Ambient pressure dried hydrophobic silica aerogel monoliths were prepared via simultaneous solvent exchange and surface modification in order to minimize volume shrinkage and density. At room temperature, the obtained silica aerogels had a low density of 0.096 g/cm³, a high surface area and hydrophobicity, and a low thermal conductivity of 0.0217 W/m·K. The effect of heating on these properties was also determined. After the aerogel had been heated to 300°...