Thermal conductivity and mechanical properties of aluminum nitride filled linear low-density polyethylene composites

The objective of this study was to create polymer composites with high thermal conductivity and mechanical properties. To acquire these, aluminum nitride microparticles were modified with a titanate coupling reagent of isopropyltrioleictitanate, and blended via a power-mixing method into linear low-density polyethylene. Using a thermal constants analyzer, the thermal conductivity of the composite was measured. The results concluded that the addition of aluminum nitride particles to the composite enhanced the ...

Author(s): , , , ,