The Effect of Cu2O Nanoparticle Dispersion on the Thermoelectric Properties of n-type Skutterudites

This article studies the effect of dispersion of Cu2O nanoparticles on the thermoelectric properties of Ba0.4Co4Sb12 and Sn0.4Ba0.4Co4Sb12 skutterudites. It was found that the dispersion of these nanoparticles resulted in an increased thermoelectric efficiency due to decreased electrical resistivity ...